Ironderero:
Umutungo | Ingingo yoroshye˚C | ViscosityCPS @ 140 ℃ | Uburemere bwa molekuline Mn | Agaciro Acide | Ibara | Kugaragara |
Ironderero | 130-135 | 8000-10000 | 4000-5000 | 20-30 | Cyera | Ifu yera |
Inyungu y'ibicuruzwa:
1. Irashobora gukoreshwa nka PVC nandi mavuta ya plastike.
2. Amavuta meza yo munda no hanze.
3, Irashobora kunoza amavuta hagati ya polymer nicyuma.
4, Irashobora kunoza ikwirakwizwa ryamabara.
5, Tanga ibicuruzwa neza no gukorera mu mucyo.
6. Nibyiza kunoza umusaruro